1FAILURES AND THE LIFE OF FURNACE TUBES显示文摘It is showed after the furnace tubes serviced for 8-10 years that the density of damage in the HAZ (heat affected zone) of the weld has higher than in parent metals, though the depth of damage is not equal to. By the test of creep crack growth, it is also acquired that under same mechanic parameter C* (t), the rate of creep crack growth in the HAZ is more than twice as fast as in parent metals. Two mechanisms (overheating and thermal shock) of failure occurred in an accident are presented. The stress of thermal shock is analyzed, in which the change of the elasticity modulus with the radius ET = f(r) is considered. Based on it, the safety region of the thermal shock is obtained. Finally, two sets of curves for the safe life are suggested which can facilitate to estimate the remaining life of HK-40 or HP-Nb tubes by their creep rupture data.F.Z.Shen Y.Ding D.M.Hou Z.P.Ning Y.Lü T.B.Dong A.R.Tuohuti 2004Acta Metallurgica Sinica(English Letters)2004,17,4:0
返回顶部 每页显示:
共1页 首页 上一页 第1页 下一页 末页 /1 跳转

网站首页 | 关于我们 | 联系我们 | 产品服务 | 客服中心 | 广告服务 | 版权声明 | 网站联盟 | 友情链接 | 售卡网点

版权所有© 渝B2-20050021-1 渝公网安备 50019002500403号 违法和不良信息举报中心

互联网出版许可证 新出网证(渝)字10号 全国400电话 - 免长途话费