    题名 作者 年代 出处 被引量
1USING HIGH Mg-CONTENT CORED-WIRE TO SPHEROIDIZE AND DESULPHURIZE DUCTILE IRON MELT IN INDUSTRIAL EXPERIMENTS显示文摘Mg-content cored-wire was used to desulphurize and spheroidize ductile iron melt in industrial experiments. The optimal feeding speed and suitable treatment temperature were determined in the experiments. And cored-wire method and pouring method were compared. Conclusions have been drawn that, under these conditions in the experiments, the optimal feeding speed is 15m/min, treatment temperature should be as low as possible, 1400-1450℃ generally; and cored-wire method can act more effective in ductile iron melt desulphurization and spheroid than pouring method.R.Z.Wu B.D.Sun H.J.Ni Y.B.Wu H.S.Wu J.G.Ge 2004Acta Metallurgica Sinica(English Letters)2004,17,6:2
2REMOVE INCLUSIONS FROM ALUMINUM MELT INELECTROMAGNETIC FIELD显示文摘Electromagnetic separation of non-metallic inclusions from Al-Si melt is studied by theoretical analysis and experiments on self-designed electromagnetic separation apparatus. Metallographs and LECO Image Analysis System were used to analyze the content of alumina in aluminum alloy before and after electromagnetic separation. It is seen that removal effciency increases with the increase of electromagnetic force (EMF) and diameter of inclusion particles while decreases with the increase of melt velocity and height of separator. All alumina particles with diamete of 14μm have been removed successfully from the melt.T.X.Li Z.M.Xu B.D.Sun D.Shu Y.H.Zhou 2000Acta Metallurgica Sinica(English Letters)2000,13,5:0
返回顶部 每页显示:
共1页 首页 上一页 第1页 下一页 末页 /1 跳转

网站首页 | 关于我们 | 联系我们 | 产品服务 | 客服中心 | 广告服务 | 版权声明 | 网站联盟 | 友情链接 | 售卡网点

版权所有© 渝B2-20050021-1 渝公网安备 50019002500403号 违法和不良信息举报中心

互联网出版许可证 新出网证(渝)字10号 全国400电话 - 免长途话费